How to Hold Tolerance on Anodized Aluminum Parts

Close-up of a stainless steel dial caliper with a yellow measurement dial checking the internal diameter of a machined metal component.

Your 6061 housing measured perfectly on the CMM. Two weeks later it comes back from hard anodize, the bearing bore is tight, the slip fit now presses, and the whole lot is on hold. Nobody machined it wrong. The size was right for bare aluminum, not for anodized aluminum parts.

The benefits of anodizing aluminium are well known, but the coating grows into and out of the surface at the same time, so every machined feature moves after it leaves your shop. In this post we break down how much each anodize type changes a dimension, how to set pre-anodize sizes for bores and outside diameters, and which drawing notes stop the argument between machinist, anodizer and inspector before it starts.

How Much Anodizing Changes a Machined Dimension

Anodize is a conversion coating, not a layer of paint. Part of the oxide grows outward and part penetrates into the aluminum, and the Aluminum Anodizers Council puts hard anodize at 50 percent penetration and 50 percent buildup per surface. Only the buildup shows up on your gauges.

    • Type II (sulfuric): 0.0002 to 0.0008 in. total thickness, with roughly half of it as buildup per surface.
    • Type III (hard): 0.002 in. nominal thickness, with about 0.001 in. of buildup per surface.

Actual thickness varies with alloy and process, so ask your anodizer for their real number rather than working from a chart.

How to Set Pre-Anodize Sizes for Bores and Outside Diameters

A diameter changes by twice the buildup because the coating grows on both sides. Bores and slots get smaller, while shafts and bosses get larger.

    1. Get the anodizer’s target thickness and tolerance in writing.
    2. Halve it to find the buildup per surface.
    3. Double that for every diameter, then open bores and reduce outside diameters by that amount.
    4. Tighten the machined tolerance band so coating variation still lands inside the finished tolerance, and use our CNC tool runout guide to keep the spindle from eating that margin.

For example, a 0.5000 in. finished bore with 0.002 in. of hard anodize should be machined to 0.5020 in.

Which Features Need the Most Anodize Allowance

Some features absorb coating variation easily. Others fail inspection on the first part.

    • Bearing bores and press fits, where coating variation can use up most of the tolerance and precision carbide reamers earn their place.
    • Slots and keyways, which close up by twice the buildup, just like a bore.
    • Stacked assemblies, where a five-part stack has ten coated faces adding height.
    • Threads, where pitch diameter moves even more than a plain bore and a standard tap will not leave enough room.

Drawing Notes That Prevent Anodize Disputes

Most anodize tolerance problems start on the print. If the drawing does not say when a dimension applies, the machinist, anodizer and inspector will each assume something different.

    • State whether dimensions apply before or after anodize.
    • Call out anodize type, class and thickness range to a named spec such as MIL-PRF-8625.
    • Identify every masked feature.
    • Define which features are inspected before parts ship to the anodizer.

Plan the Allowance, Then Hold the Size

Anodize allowance is simple math, but it only works when the bare part lands exactly where you planned. Once a hard coat uses up part of a bore’s tolerance, the band left for your shop is narrow, and tool deflection, runout or a worn reamer edge can push a part outside it before it ever reaches the tank. That is where tooling earns its keep. We grind solid carbide end mills, drills and reamers in Stoney Creek, Ontario, built to hold size part after part in aluminum. If you are quoting a tight-tolerance anodized job, contact our tooling team and we will help you match the tool to the allowance.

Frequently Asked Questions

Can anodize be stripped and redone if parts come back out of tolerance?

Yes, but stripping does not return the part to its original size. The strip removes the full oxide, including the portion that penetrated the base metal, so bores end up larger and outside diameters smaller than when you machined them. Plan any re-anodize around those new bare dimensions before sending parts back.

Does sealing change the dimensions of anodized aluminum parts?

Not in any way most tolerances will notice. Sealing closes the pores inside the oxide rather than adding a new layer on top. The bigger trade-off is hardness, since Products Finishing reports that sealing a hard coat can cost up to about 30 percent of its hardness. Specify unsealed hard coat where wear resistance matters most.

How do I measure coating thickness on a finished anodized part?

Use an eddy current coating thickness gauge, which reads the oxide on aluminum without damaging the part. Comparing micrometer readings taken before and after anodize also works, but that only shows buildup, not total thickness. For disputes, ask your anodizer which method their certification is based on and match it.